Effect of addition time on recarburizer

Recarburizer is widely used in steel making and casting to adjust the carbon element, in the use of recarburizer added time on its impact is quite large, directly affecting its utilization rate and the benefits of manufacturers.

Effect of addition time on recarburizer

It is especially important to master the time of adding carbon additive, many factories will appear to add carbon additive too early, so that part of the carbon additive adheres to the bottom of the furnace, and some of the carbon additive attached to the inner wall of the furnace will not be melted, thus reducing the absorption rate and utilization rate of carbon additive.

Want to properly control the time to join, you need to add recarburizer in small amounts several times, so that you can better control the amount of recarburizer added. It is a good choice to consider the addition time of carbon additive in combination with the heating temperature of induction furnace, which can ensure the absorption time of carbon additive in the iron solution is about 10 minutes. In addition, if you want to increase the absorption rate of the carbon additive can also be stirred to make the carbon additive fully dissolved and absorbed, which can also effectively reduce the nitrogen content in the carbon additive and improve the fluidity of the molten iron.

LEAVE US A MESSAGE

*